The only real change between my last post and this one is getting “the filter” printed, assembled, and running. This doesn’t seem like a print that would be prone to warping, so it’s probably not a great test, but I am trying brimless. I can feel a decent amount of heat coming off the enclosure, so it’s certainly warmer in there than it has been in the past.
Next: try going faster! This is an 8 hour print using basically the stock superslicer profile for the 350 2.4. I did bump up extrusion width, but flow rates are still very low compared to what my rapido HF should be able to deliver with ASA at 250. I’m thinking that I should try the same speed for both internal and external walls. That would save me 2 hours. Maybe I should just go with a larger nozzle? I don’t want to decrease wall count, not that is even practical on this model.